한국표면공학회지 (51권5호 291-296)
Corrosion Damage Characteristics with Materials and Process Time in Ultrasonic-Chemical Decontamination of Immersion Type
침적식 초음파-화학 제염 시 재료 및 공정 시간에 따른 부식 손상 특성
이승준;현광룡;한민수;김성종;
Lee, Seung-Jun;Hyun, Koangyong;Han, Min-Su;Kim, Seong-Jong;
군산대학교 해양과학대학 마린엔지니어링전공;목포해양대학교 해군사관학부;목포해양대학교 기관시스템공학부;
Department of Power System Engineering, Kunsan National University;Division of Naval Officer Science, Mokpo National Maritime University;Division of Marine Engineering, Mokpo National Maritime University;
In this study, we carried out an ultrasonic-chemical decontamination process with immersion type, reproduced in the laboratory. The corrosion damage characteristics, depending on kind of materials and ultrasonic process time, were investigated. Inconel 600, which showed lower corrosion potential and higher corrosion current density than that of STS 316, revealed severer corrosion damage and higher weight-loss rate than STS 316. Weight-loss rate of Inconel 600 increased with increasing ultrasonic process time. On the other hands, STS 316 presented a negligibly small corrosion damage, which was almost indistinguishable from visual observation. There was no effect of ultrasonic process time on the weight-loss rate of STS 316.
Chemical decontamination;Ultrasonic process;Corrosion damage characteristics;STS 316;Inconel 600;